Picture Name
You can consider 4 factors
A)Moisture: if moisture of gas is over 10% and desiccant can’t be loaded in the purification system,you can choose XT-051 and XT-CAT-01G.
B)Airflow: if airlow is over 10000 M3/h. It’s better to choose XT-051. Honeycomb can reduce air resistance.
C)Lifespan: In the environment with a certain humidity ,If you want lifespan over 2 years. It’s better to choose XT-CAT-01G. It has added precious metal Pd or Pt, featuring water-resistance.
D)Application, For gas mask, popular solution is XT-CAT-01, but it should be used together with desiccant. 
If it’s used for dry gas, XT-CAT-01 is also the best solution because it’s cost-effective. For more details,Xintan team can offer professional advice.

Picture Name
Ingredients and Carrier are different.

Picture Name
Based on GHSV and Airflow,we can calculate the required volume of catalyst.

Picture Name
Different customers have different working conditions.Before placing bulk order, you can test sample.